View Single Post
  #1 (permalink)  
Old 04-27-2006, 10:16 PM
Canute7 Canute7 is offline
Newbie
 
Join Date: Apr 2006
Posts: 43
Canute7 is on a distinguished road
Default colors coming out light

hi guys,
I've started having some problems, things seem like they should be working, but not quite my colors keep coming out light, I just did a piece that I dyed dark red and it came out a mettalic pink, 3 pcs (at once) came out very light pink.
My gut tells me it electrical, seems that I'm not getting the amperage that I should, but my power supply says its putting out the set amount(varies, of course), is this just a bad connection or is there something I'm missing?
Thanks
Canute