Default Re: colors coming out light

SS, my amps move around usually+/- .01, for instance the last part was 6.5 sq in. CD was 4.5, 720 rule said use .20 amps. My read out would move from .2 to .19 or .21, my voltage started off at 4.5V and during the run it moved to 11.1, W/ the 720 rule saying 11.25 I didn't see this as a problem. I ran my part for 80 mins to get .5 mills.