Originally Posted by Shaw_2112
Got a new chrome peice for my bike in the mail and it had some strange dark discoloration on it. I took a loose wheel with some blue compound and polished it out, it took a little bit but it finally came out, however it left some very fine micro scratches in my chrome. Is there anyway to get my mirror finish back or am I just going to have to live with it? If it wasn't a new piece I wouldn't even care, very hard to see unless the light hits it just right, but it is a new piece and I'm a little dissapointed in myself for messin it up.....
|
Try a canton flannel wheel and a lower speed.