It does take away some of the reflectivity, there's no getting around that. There is "another" manufacturer that sells Single Stage Reflective Chrome, doesn't need a clear coat, so it stays reflective.
No, I don't normally use a primer unless the part is continuously out in the weather. Most of what I do is Custom cars, hot rods, bikes, sleds. Most of them are stored indoors.