View Single Post
  #4 (permalink)  
Old 04-29-2006, 01:37 PM
ShelbyCSXT's Avatar
ShelbyCSXT ShelbyCSXT is offline
Amateur Metal Finisher
 
Join Date: Apr 2006
Posts: 97
ShelbyCSXT is on a distinguished road
Default Re: Powder crawls away

It sounds to me that the static cling thing isn't working in those spots. At this point, it looks like you don't want to strip it down to bare metal, so i'd suggest heating it up to 150f and shoot it while it's hot. From what i understand, you'll see the powder melt on contact, so it wont matter that you cant get the static cling.