Re: Why does my math not jive with 720 Calculator?
I appreciate your time SS. As I am currently running out the door (to carry a washing machine into my sister-in-law's basement of all things), I don't have the time right now to look over your response. Before I go, if you haven't answered this already, I have a question for all :
Using an electrolyte with a 9.4% (by volume) sulfuric acid contend and a temperature of 70F, if I were to use a current density of 12 amps to anodizing a part, what it the calculated PAR?
Thanks for the help...
|