RedRiver is on a distinguished road
Send a message via MSN to RedRiver
Default Re: Why does my math not jive with 720 Calculator?

I suppose a surface area is required in my above question, so to add to my above post (since I can't seem to edit it) :

Using an electrolyte with a 9.4% (by volume) sulfuric acid content and a constant temperature of 70F, if I were to use a current density of 12 amps per square foot to anodizing a part with a surface area of 1.75 square feet, what would be the calculated PAR?

If you are able to, please show me in longhand your mathimatical answer.