Are the problem parts fresh buffed. The way I've found that works best for mine is to clean in naphtha (Varsol) with a toothbrush, then with Dawn dish washing liquid in a heavy concentration. The parts usually always pass a water break test but if they don't, I just go back over them with the detergent.