Hi everyone, thanks for the input.
Just got back from the barn, did my first 2 color part, dark red/fast blue. It came out great !!!!!! I touched it with my bare hand, so I got a fingerprint on it , but I'm still thrilled w/ it!!!!!!!! I used plast-i-cote high heat to mask w/, I had to use laquer-thinner to get the paint off(coudn't find 500 degree, used 1900 degree), but came out great!! My colors came out nice and dark, I left a band about .25 in unmasked, this turned a dark purple, of course. I can't wait to see it in the sun, looked cool in the light in the barn.
I will be doing my first "real" part next, might be a couple of days before I can, will keep U all updated.