Quote:
Originally Posted by azoldbill
I am no expert, but I did a brass plate with silver vein and got the "small" effect you described. I then did an aluminum framework and went a bit heavier with the coating and got a notably courser texture. My theory is that the more powder you build up, the courser the texture, but I'd like to hear it from others to be sure that my observation isn't flawed.....

that was my guess but all i've done so far is a small 2" alumunum sample.

Anybody know anything about the high temp? Should it be pretty smooth and glossy compared to a normal powder? I'd really like to try and redo this piece tomorrow.
__________________
Unorthodox Creations Powdercoating