Default Re: colors coming out light

SS, I think I just got it right, good connection, I also bumped my amps to 6amps/sq ft, this seems to have helped the lightness issue. I was a little worried this part didn't act like any of the others, volts shot right up to 17.1V, and then slowly moved down to 16.1V thru out the run(2hrs), but it came out great!!
C U later,
Canute