Well...Curiousity killed the cat and I just had to try it...Here's my 2K3 System-X Autococker with it's new polished red & black acid wash anodizing. I figure it turned out pretty well.
The eBlade trigger frame and the solenoid cover where initially chrome plated. After some experimenting and tons of reading I found may way around that. I didn't do the barrel (yet) because I have a new Freak Kit for it that I want to do but ran out of time. The rest of this marker was bead blasted and a matte boring black. What a facelift!