Default Re: Acid Wash for header prior to Ceramic Coating

Im sure this post is going to really help alot of people. If anyone has more of an idea on how the "bathing" process works, it would be appreciated. Do you soak, if so, how long? Do you spray or ?? Does it need to be heated? How long will the dilution last? Can it go in a plastic barrel or metal or ?? If anyone has a procedure or something on how it works, that would be great. As well, if anyone recommends a phosphate bath and how that works.


p.s. Thanks for the tip on MCS...I was just about to coat the inside with the black satin...Yikes!!! Do you worry about getting any on the outside or is that OK?