Quote:
|
Originally Posted by Timmer
p.s. Thanks for the tip on MCS...I was just about to coat the inside with the black satin...Yikes!!! Do you worry about getting any on the outside or is that OK?
|
Being that I have yet to use any of the stuff, you might wana ask/email the company and don't trust my word as being the ultimate decisive factor. But the
MCS description says:
* Extreme temperature capable (2000f +)
* Water based coating, no VOC’s
* Use under any TECH LINE exhaust system coating to increase
* the temperature that the top coating can withstand
* Use in pipe I.D. as well as O.D.
* Improve exhaust gas velocity, increase H.P.
* Requires Baking. Cures at 500f. Must be oven cured
MCS runs $102 per quart(32oz), versus Black Satin's $55 per 1/3 quart(12oz). The MCS is sold only to people with a business license, etc.
Hope this helps