I'm a fan of the polypropylene myself. Easy to weld and holds up nicely. My tanks are 1/2 thick PP sheet which I cut and welded into 45 gal tanks. Ran PP ribs around the top and middle of the tank and they are strong, strong, strong!!

Just my $0.02