View Single Post
  #8 (permalink)  
Old 05-08-2006, 11:26 PM
FSTFBDY FSTFBDY is offline
Amateur Metal Finisher
 
Join Date: Mar 2006
Location: Ohio
Posts: 94
FSTFBDY is on a distinguished road
Default Re: Acid Wash for header prior to Ceramic Coating

I have a 55g drum of muradic. I blast all my headers 1st to get rid of rust and as much of the carbon I can. Then just soak em and go do something else for a few. sometimes 5min. some times more.