Quote:
|
Originally Posted by FSTFBDY
I have a 55g drum of muradic. I blast all my headers 1st to get rid of rust and as much of the carbon I can. Then just soak em and go do something else for a few. sometimes 5min. some times more.
|
What concentration do you use Chris?