I use a bit of sponge... either natural sea sponge (which will be eaten up) or some synthetic sponge.
With gloved hands, dip the sponge, then squeeze out the excess... you don't want to drip bleach or acid where it's not wanted.
__________________
Specializing in anodized graphics in Paintball guns.