Default Re: Machine Polished Lip?

Quote:
Originally Posted by pikkashoe
Also what are you thoughts on the wax and causing more scratching and now what looks like clouding or haziness. I used a carnuba paste wax. I might just forego this step and just finish at canton flannel with red rouge.
A good wax shouldn't cause scratches! Try using brake cleaner or acetone to clean the aluminum prior to applying the wax. The haze could also be caused by not enough temperature in the aluminum when buffing.

John