View Single Post
  #5 (permalink)  
Old 05-12-2006, 10:11 AM
neromich neromich is offline
Newbie
 
Join Date: Feb 2006
Posts: 7
neromich is on a distinguished road
Default Re: flash copper and copy chrome help

I am going for a satin finish on the entire head. So I thought that needed to be done on the copper. Maybe I was just to aggressive with the bead blast.
Reply With Quote