Originally Posted by Livinincolor
The one problem I do know about is you cannot spray powder coat over a part that is already coated.

The already cured and hardened powder does not seem to conduct the charge needed to attract the new powder.

Please be careful when giving advice. Its obvious you have not been pc'ing for very long, because you are WAY wrong. You can easily do multiple coats... multiple, not just two... but 3 or more. Thats they way people get all the trick looking colors and textures.

You are right that the existing powder does not conduct... its not supposed to. The part is. Thats why you need to make sure the ground is good.