well i just got donw doing a few parts,
and sprayed the Extreme chrome, cured at 395, for 15 min, let cool then sprayed a thicker coat of clear then cured for 20 min,pulled it out and the sweet chrome had turned in to a mirror silver or the like,
should i make sure i fully cure the 1st coat? what did i do wrong any input would be great
thanks,
Jesse