Re: Extreme Chrome with Clear Coat How to...
With the chrome powders you must fully cure the chrome powder before the clear top coat. As Jim stated in the first post let the extreme chrome cool all the way down to room temperature the coat with clear. I have done this with super chrome and exterme chrome with great results. The silver effect is definately from under cure I have done the same thing myself.
JASON
|