View Single Post
  #6 (permalink)  
Old 05-16-2006, 02:37 PM
kenrinc kenrinc is offline
Newbie
 
Join Date: Dec 2003
Posts: 31
kenrinc
Default Re: Too much brightner?

Sean,

I do think that I need better wiring (thicker). I'm just using standard test cables and normally they just connect to the wire. For the caliper I think I may actually connect it to the part. Is it better to fully emerse the part wire in the electrolyte or have it connect to a wire that connects to the part? It seemed to plate better with the clip directly in the electrolyte.

Something happened last night when I tried to add some top up water to the bath: when I poured the dist water in the bath, it "gelled" up. It was weird. Almost like egg on the top of soup. I mixed it around and it seemed to go away but left a haze in the tank. I've ordered more electrolyte. Wish I could figure out what the problem is.

Ken-