Default Re: Too much brightner?

Ken:

This is typical of some power supplys. They will not operate into low resistance loads. As you add more anode surface area, you're decreasing the resistance within the electrolytic "cell" (which is what your electrolyte tank is).

Put a 1 ohm high wattage resistor in series with the positive lead and it should work.