Default Re: Too much brightner?

Ah. Got it. I've got a 1 ohm, 10 watt unit I can try. Seems like a small wire for such large current though. I've got some pics of what I've gotten so far, I'll post them later. Since it looks as if I only had one or two anodes hooked up for any span of time it would plate on one side only and then only on high parts of the part. I'm still dumbfounded on how to get a better idea of the surface areas involved. 12amp seemed like the right amount of current but after looking at it again it might be too much as the plate was rough in most of the areas it went down.

It's funny, I've used the bath to plate a plethora of smaller parts yesterday with no problems at all! Large parts are a definite learning experience for me!

Ken-