I tried w/ Picklex, then without. No real difference in appearence. Haven't done the phosphate coating.

This is all after degreasing, sandblast, blowoff (3 stage filter dryer), and wipe down w/ acetone. Also tried spray off w/ non-residue brake cleaner instead of wipe w/ acetone. No difference.