mirror red q's
before i found this site i bought a competetor's set up. With it I got the ******* system and mirror red, black, and blue. After playing with the silvervein and coppervein, I decided to spray the mirror red. I thought it was a kandy coat but when i put it over my polished part is turned to a regular none transparent red. Did i possiblly spray to much powder? I stayed 6" from the part and adjusted my air regulator at the gun to 8-10 psi. I then let it flow out at 450 for 7 min, and then final baked at 400 for 20 min. This is what the directions say to do. Where did I go wrong? Any help please
|