Hi, I'm trying to repair a few scratches in the crome car bumper. They are all the way down through layers of plating, some really narrow, and some up to about 1/4 inch wide, and starting to rust a little. I purchased a Plug N' Plate kit with both Copy Chrome and Copper solutions, and was planning to fill the scratches with copper first, then sand and buff and plate with Copy Chrome. Or will soldering iron and some solder be better for filling the scratches before plating? How thick of a copper layer can I build with this kit? Any pointers on how to do it the best way?