the schedual was
15 min in stripper
polish
5 min cleaner @ 137 degrees
3 min desmut room temp~61 degrees
1hr ano @ 15v/6amps/63 degrees
10 min dye @ 139 degrees
20 min sealer @ 161 degrees
krymis