Re: When the power goes out?
it wouldnt be ok to leave them in the acid especially for 5 h for the power to come on and lets say another hour for the ano to finish. You will badly pit your parts.
Ive never had such a problem but I would take the parts out, rince them and continue the run when the power gets back on.
|