Nope just home use. He owns the weldshop that had all the equipment to build my oven so I dont mind coating stuff for free for him. I coated them tonight in Bright White. He's getting the coolant system checked out just to make it isnt leaking anywhere then it will be up and running. He had it down to 10 degrees F a couple nights ago so I'll get to check out pieces at least that cold and see how well they hold up.