Originally Posted by pickleboy
i wet sand with alum oxide all the time and never had a problem. it may have to do with the paper manufacture.
You know, it's funny. I went to the store and got some REALLY sticky velcro. I took some of my wetsand sandpaper and cut them to the size of the mouse. Sticking it on the bottom, using a squirt bottle, I don't see any difference other than it's taking me like 20 min... instead of 2 hours to get the same amount of work done. The valve cover I'm working on is going a LOT faster. I even used duct tape to roll under the sand paper to get it to stick, and it works like a charm. I guess you just have to work with what you got. I'll use the pads that I have for the mouse on other projects. Squirting the vavle cover, and THEN sanding, works pretty well.
Reply With Quote