Re: quality of Anodiz....
parts ran in larger part runs seem to be less durable, also parts people do on their own and stripped down are usually done in a short amount of time, where as Ano's from a factory sit for 6-8 months probably before the part is stripped by you and is drained of the excess light oils and such used to restore oil to the surface, like WD-40
Just more guess'es
|