Quote:
wildting wrote:
How corse would you reccomend? 320 or should I go the 400, 600 and then the polish wheels or do I add the 1000 in there too?

Thanks,
J.P.

Wildting, I wouldn\'t mess with the 320. 400 should do it pretty good. just go over the pitting well. Without viewing it not really sure, but 400 should be able to do it.