The main difference I noticed starting out with a 3 gal. and moving up to 15, 20 gal was the amount of heat the tank could handle. I never really noticed anything else. I used aeration up to the 20 gal. The first tank was a square plastic cat food bucket. It worked well, I just outgrew it on the size of parts I was doing. If the parts you do are small enough to go in the tank with enough clearance to the cathode you probably won't notice any differences.