Default Re: Small tank anodizing

Quote:
Originally Posted by caswellsage
From where to where did you measure that.
I attached short Ti wires to my test leads and stuck them into the bath about 1/8" depth. It was when you'd said something about high resistance of a weak acid solution, so I was curious about the resistance of the solution itself, as opposed to the overall resistance of a part being in the solution. In and of itself I don't think the number is useful for anything; just general curiosity.

I have my plates set up so that I can move them in response to part size.


Quote:
Originally Posted by destroyer125
upgrading from a 2 to 10 gallon tank ive noticed heat will not fluctuate
So it's looking like going the other direction I may have some problem with temperature but no other surprise issues.