View Single Post
  #4 (permalink)  
Old 05-27-2006, 04:22 PM
destroyer125's Avatar
destroyer125 destroyer125 is offline
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 444
destroyer125 is an unknown quantity at this point
Default Re: Setting up a 20 gallon sink

Im not sure if your water around your cooling coils will be cold enough to affect the temperature of the acid, Im having trouble cooling my tank overall with 60* water to the 80* tank, but if I cool the water down to the 40*'s it will begin to affect the acid tank