ok my lollypop red turned orange when i applied super high gloss clear to it. It was applied to an engine pulley.
All products are caswell:
lollypop red
super chrome
super high gloss clear
my spray schedual is this:
shot super chrome at room temp, cured at 435 til flow out (approx. 5 min) then down to 400 for 10 min.
-turned out fine other than bumps which i guess are outgass pockets
shot lollypop red on part at 150 degrees, cured at 435 til flow out 9approx. 5 min)and then turned down to 400 for 10
- looked great except for the few sags at the lowest point
shot the super clear on part at 150 degrees , cured at 400 til flow out then down to 392 for 15 min.
-part turned orange and needed to be stripped and redone.
Any help please.
|