I just bought a copy chrome kit. when i set it up and began to chrome;I started having problems. I later found out that i had too much current going to the part. causing the part to be black and crusty. When this happens will it ruin my solution? then after that happened i got flustrated and hooked the +/- backwards for about thirty minutes. i haven't attempted to chrome anything else. can someone help me?
thanks jeremy
|