Re: Setting up a 20 gallon sink
Currently I have a larger tub around my tank that I put 2 gallons worth of ice in the tank and within 30 minutes it will drop the tank down to about 72, and stay there, Im thinking about trying dry ice also, I will be upgrading to a chiller before winter hits and Will keep my tank at 68* if the chiller can do it
|