retrofitting an agitator
i have a Clarke SB9006 blast cabinet and would like to retrofit an agitator to it. Any ideas? I have no idea how they work or what they are. Also i have excessive media coming out of the lid area. I checked the seals and they are good and I checked the latches for the lid and they are tight. I am not running any vac to it and i have the foam filter in the back inlet and a cone filter on the vac hook up/oulet.
|