well think by god i got it. I did the pulley out side of my booth while still hot from the oven on the reheat. It temped at 271. I sprayed the red with just a light dusting and BAMMMMM(in my best emeril)...no runs sags or anything. THe bracket got ground down again and is chromed and red waiting cooking. If this works out I will be doing a valve cover tonite.
|