Quote:
Originally Posted by Livinincolor
Did you prep them properly?
Did you do a pre-PC burn off?
Did you try pre-heating them right before PC'ing?
Johnny
Sho Me Coatings
1. Yes
2. What? If you are referring to outgassing it is machined cold rolled steel that shouldn't need outgassing. It doesn't show any signs of outgas anyway, just a rough finish that is comparable to "dryspray" in the automotive painting world.
3. Yes
Anyone else have any thoughts?