Default Re: Questions on PCing HD wheels

Firt I would heat the wheel to 425 to help remove the polish from the wheel or at least wipe down with Acetone. Once done tape what you do not want black and shoot the black then clear. No you do not need to clear coat the black and it will not hurt it either.. So tape and PC...

Jim S...
__________________
Jim Shuster
www.backyardpowdercoating.com Sold.....
www.chrissys68mustang.com Hobbie
www.photogserver.net Web Hosting.