Thread: Gun cleaning
View Single Post
  #1 (permalink)  
Old 05-31-2006, 11:58 AM
gcastor gcastor is offline
Newbie
 
Join Date: May 2006
Location: New Hampshire
Posts: 18
gcastor is on a distinguished road
Default Gun cleaning

Hi everyone. New guy here. This forum is great. I have learned alot by reading what everyone has experienced. I have a problem that I did not see anything on and that is gun cleaning. I used a white gloss PC on a part the other night. Shortly before that I used a red color. My second part had red specks all thru the white after my bake. I used compressed air to blowout every hole I could find repeatedly to ensure I had a clean gun before I changed colors. Does anyone know of anything else I can do to clean my gun better? This is really frustrating me. Thanks Greg
Reply With Quote