View Single Post
  #7 (permalink)  
Old 05-31-2006, 03:40 PM
jimcarry's Avatar
jimcarry jimcarry is offline
Experienced Metal Finisher
 
Join Date: Jul 2004
Location: Arkansas
Posts: 370
jimcarry is on a distinguished road
Send a message via Yahoo to jimcarry
Default Re: CC and Plastic Model Kits

The reason you would use the acid copper over the silva spray is because the silva spray has small pieces of silver in it the acid copper will give you a smooth finish I have seen it on some hot wheel cars and it looks great the copper conductive spray you are talking about I have not used before but I would give it a try see what happens use test piece
__________________
Jim Eaton
Reply With Quote