Smile high temp. cement?

Hello everyone,
I am NEW to powder coating, I have taught myself, with help from guys on this fourm to annodize, so I figure this is a good place to learn to powder coat!!
Now to my question. Have any of U guys tried the high temp cement that is sold at McMan-Car? Do U see any problem with this if the oven is NOT moved or at least not much?
I was thinking that U could coat the INSIDE of your oven, as it is rated to +2300*F, this might let U do away w/ the outside box, what do U think?
ALL suggestions/replies welcome.

Thanks
Canute