Quote:
|
Originally Posted by gcastor
Hey guys, i happened to have a scrap atv resorvoir hanging around and tried it. The window held up right to the last 5 mins of my cure then it started to whiten and bubble. If you can get it out, take it out
|
This is awesome! Thanks for trying this. We will try to remove the sight glass and I will post the outcome also. My friend at a local machine shop said he can make a tool to remove these

. If it works and he can make these reasonable enough I will possably offer a few if anyone wants one.
Jason