Re: Can you figure out what I did wrong?
cruizer,
First why are you using a Gease/wax remover? You did say you are outgasing correct? if so just use Acetone as a wipe on or from a spray bottle.
The less you put on after it has been Outgassed the better.
Steps:
Sandblast, Spray with cleaner, outgas, cool then powder..
Jim S...
|